Axial solution precursor plasma spray (SPPS) has recently emerged as a promising route for producing highthroughput, strain-tolerant yttria-stabilized zirconia (YSZ) thermal barrier coatings (TBCs). The mechanisms governing their degradation under prolonged high-temperature exposure remain unexplored. In this study, the evolution of the coating microstructure, mechanical properties, and delamination behavior was investigated during isothermal exposure in air at 1150 degrees C. Enhanced thermally grown oxide (TGO) growth in axial-SPPS coatings drives a distinct delamination pathway. Prolonged exposure results in the formation of a multilayer TGO consisting of laterally continuous alumina (Al2O3) and chromia (Cr2O3) sublayers, reaching a total thickness of approximately 20 mu m at 200 h. This TGO thickness is significantly higher than typical values reported for SPS and EB-PVD coatings under broadly comparable time-temperature exposure conditions, where the TGO is usually dominated by Al2O3. The results indicate that the macroscopic delamination after 200 h exposure is associated with the coupled influence of vertical crack morphology and the multilayer TGO. Vertical cracks act as initiation sites for delamination at the TBC/TGO interface, while the Al2O3/Cr2O3 interface facilitates sustained crack propagation and large-scale coating delamination. These results provide new insights into the microstructure-delamination relationships relevant to the durability of axial-SPPS TBCs.
CC-BY 4.0